Insulation Type | Thermal Conductivity | Vapor Barrier | Water Absorption | Tensile Strength | Shrinkage | Fire Proof Rating |
Irradiation Polythene Insulation (IXPE Insulation) |
≤0.033W/m.k | u≥5000 | ≤0.0076 g/100cm2 |
≥0.34MPa | ≤7% | ASTM E84 UL 94 AS/NZS 1530.3 EN 13501-1 |
Copper Alloy | Chemical Composition | Temper | Mechanical Property | Grain Size mm |
||
Copper % |
Phosphorus % |
Tensile Strength MPa |
Elongation % |
|||
C12200 | ≥ 99.90 | 0.015-0.040 | O60 | ≥ 205 | ≥ 40 | ≥ 0.040 |
C12200 | ≥ 99.90 | 0.015-0.040 | O50 | ≥ 205 | ≥ 40 | 0.015-0.040 |
Copper Alloy | Chemical Composition | Temper | Mechanical Property | |||
Copper % |
Phosphorus % |
Tensile Strength MPa |
Elongation % |
Hardness HV |
||
Cu-DHP | ≥ 99.90 | 0.015-0.040 | R220 | ≥ 220 | ≥ 40 | 40-70 |
Copper Alloy | Chemical Composition | Temper | Hardness HV |
Grain Size mm |
|
Copper % |
Phosphorus % |
||||
C12200 | ≥ 99.90 | 0.015-0.040 | O | ≤ 75 | ≤ 0.065 |
Copper Alloy | Temper | Cleanness | Standard |
C12200 | O60 | ≤ 38mg/m² | ASTM B280 / EN 12735-1 / AS 1571 |